PVC Tin Stabilizer CST-128
PVC tin stabilizer CST-128 qulity is close to the 19% methyl tin mercaptide stabilizer, but the price is reduced by 20%. It can replace the popular PVC methyl tin stabilizers like SW-977, YT-181, TM-181 and other models on the market, helping factories reduce production costs.
It is suitable for manufacturers who require long machine running time and high shrink film quality.
PVC Tin Stabilizer CST-181
PVC tin stabilizer CST-181 is the cost-effective model used by most printing film and label film factories. This model has been used in the Chinese and international markets for many years. If the factory has a perfect formula and technology, this type of metal stabilizer can completely replace 19% tin.
We also provide lubricant with tin stabilizers. The coordination of lubricants and stabilizers is important.
PVC Tin Stabilizer CST-181-F
PVC Tin Stabilizer CST-181-F is used for no-printing shirnkable film,If you only produce ordinary packaging film, you can use this type of tin stabilizer.
- PVC Shrink Film Formula 1
- 2
- 3
PVC resin | 100 KG |
DOP | 4.8 KG |
Stabilizer-CST128 | 1.8 KG |
316A | # KG |
G78 | # KG |
ACR(30) | # KG |
MBS(-1) | # KG |
G53 | 1 KG |
PVC | 100 KG | |
Processing Aids | PA-20 | 0.4 KG |
P30 | 1 KG | |
PVC reinforcement | B625 | # KG |
External Lubricant | 316A | # |
96579 | # | |
Internal Lubricant | G60 | 1 |
Plasticizer | DOP | 4.8 KG |
Stabilizer | CST-181 | 1.8 KG |
Return Material | 15 KG |
PVC Powder | 75 KG | |
Podwer Additives |
K130/PA220FA | 1.1 KG |
PARALOID-K175 | 1.3 KG | |
PARALOID-BTA731/IM737 | # KG | |
OPE | # KG | |
AC316 | # KG | |
Liquid Additives |
DOP-PLASTICZER | 3.6 KG |
FINALUX-G161 | # | |
SW977/CST-128 | 1.6 KG | |
86.00 KG |
Changsheng Material
PVC Film Liquid Stabilizer CST-128/CST-181
- Specialized for PVC Shrink film, can completely replace methyltin CS-181
- Excellent thermal stability
- Cost-saving and high-quality
You are a professional in the PVC shrink film industry. A small amount of 2-5 KG cannot be used for a long-term test of a machine. We recommend a test order of at least 25KG or 220KG. You need to pay the necessary fees, but I believe that your attempt will help you save a lot of production costs in the future.
If any problems arise during the film blowing process using our PVC stabilizers and raw materials, we will help solve them. If necessary, we can arrange for technicians to go to the factory for debugging.